In vivo Study on the Corrosion Behavior of Magnesium Alloy Surface Treated with Micro-arc Oxidation and Hydrothermal Deposition.

Chuan-Yi Bai, Jian-Wu Li, Wan-Bao Ta, Bo Li, Yong Han

Abstract read
In one paragraph

Article in Orthopaedic surgery, 2017. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 2 papers.

0numbers the graph read from it
0cells of the map it votes in
2citing papers in PubMed
–field-weighted citation impact
1 · What the graph read from it

What it found

Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.

The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.

2 · The registry

The trial behind it

Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.

Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.

3 · Its place in the literature

Who cites it

2 citing papers in PubMed.

  1. Review
  2. Materials (Basel, Switzerland) · 2018
    Article
4 · The record

Corrections and comments

PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.

5 · Who and what money

Authors and funding

5 authors.

Chuan-Yi BaiDepartment of Orthopaedic Surgery, The Second Affiliated Hospital of Xi'an Jiaotong University, Xi'an, China.
Jian-Wu LiDepartment of Orthopaedic Surgery, Armed Police Corps Hospital of Shaanxi, Xi'an, China.
Wan-Bao TaDepartment of Orthopaedic Surgery, The Second Affiliated Hospital of Xi'an Jiaotong University, Xi'an, China.
Bo LiDepartment of Orthopaedic Surgery, The Second Affiliated Hospital of Xi'an Jiaotong University, Xi'an, China.
Yong HanState Key Laboratory for Mechanical Behavior of Materials, Xi'an Jiaotong University, Xi'an, China.

Funding

No grant is acknowledged in the PubMed record.

6 · The paper itself

Abstract

objectiveTo study the corrosion behavior of magnesium alloy surface treated with micro-arc oxidation and hydrothermal deposition in living animals.

methodsA magnesium oxide (MgO) layer was prepared on Mg alloy using micro-arc oxidation technology, and then a composite coating composed of magnesium hydroxide, hydroxyapatite, and MgO was coated on the MgO layer using the hydrothermal deposition method for 2 h and 24 h. Male 3-month-old white New Zealand rabbits (n = 48) weighting 2200-2300 g, were divided into four groups randomly. The prepared Mg alloy samples with composite coatings were implanted into the femoral medullary cavity of rabbits. For the Mg group, bare Mg samples without any treatment were implanted; for the MgO group, bare Mg samples undergoing MAO treatment were implanted; for the HT2h group, samples of the MgO group undergoing hydrothermal treatment (HT) for 2 h were implanted; and for the HT24h group, samples of group MgO undergoing HT for 24 h were implanted. Then the in vivo corrosion behaviors of implants were evaluated by X-ray observation, micro-CT analysis and serum Mg

resultsThe X-ray showed that samples implanted in animals were decreased as time went by. The micro-CT showed that on the fourth week, the residual volume percentages (RVP) of samples of the Mg, MgO, HT2h, and HT24h groups were 72.81% ± 2.10%, 71.68% ± 1.49%, 81.14% ± 1.54%, and 82.04% ± 0.89%, respectively; on the eighth week, the RVP of four groups were 29.45% ± 1.06%, 41.82% ± 1.13%, 53.92% ± 0.37%, and 62.53% ± 2.06%, respectively; while on the 12th week, RVP were 8.45% ± 0.49%, 9.97% ± 0.75%, 37.09% ± 0.89%, 46.71% ± 1.87%. The RVP of the HT2h group and the HT24h group were higher than for the Mg group and the MgO group for all three time points (P < 0.05); the RVP for HT24h was higher than for HT2h at 8 and 12 weeks, and the differences were significant, indicating that the degradation of Mg alloy slowed down after composite coating. In addition, the composite-coated Mg alloy by 24-h hydrothermal treatment exhibited a slower degradation than that treated by 2 h. Serum Mg

conclusionThe combination of micro-arc oxidation and hydrothermal deposition can greatly improve the anti-corrosion behavior of Mg alloy, and Mg alloy coated with this composite coating is a promising biomaterial with a satisfactory degradation rate.

Indexed as

Prostheses and ImplantsAlloysAnimalsCoated Materials, BiocompatibleCorrosionDurapatiteMagnesiumMagnesium HydroxideMagnesium OxideMaleOxidation-ReductionRabbitsSurface PropertiesX-Ray MicrotomographyAlloysCoated Materials, BiocompatibleDurapatiteMagnesiumMagnesium HydroxideMagnesium OxideCoatingCorrosionHydroxyapatiteMagnesium alloyMicro-arc oxidation

Identifiers

PMID28960817
PMCPMC6584445

What Socratic holds

Textmetadata
Read underepoch 390

Registered trials

None linked

Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the Socratic graph.